J-4040
repairRepair- Line
- LN-12
- Station
- 2424+00
- Weld date
- 2026-06-14
- Spec
- 24" × 0.375"
34.26440, -104.61240
No open cross-check alerts on this joint.
Welder passes
- RootDitch sideWeston Trahan RC-133
Jun 14, 2026, 8:35 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- RootWorking sideBrent Kessler RC-540
Jun 14, 2026, 8:35 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- Hot PassWorking sideJunior Escamilla RC-158
Jun 14, 2026, 9:10 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- Hot PassDitch sideTy Maldonado RC-552
Jun 14, 2026, 9:10 AM · logged by C. Ramirez (Survey)
WPS-1104-TI-11 Rev 1SMAW uphill 6G (fixed)E6010 / E7018-H4
4–36 in OD · wall 0.188–0.75 in · hardness 235 HV10 max
- FillDitch sideRonnie Pace RC-547
Jun 14, 2026, 9:45 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- FillWorking sideMarvin Doucet RC-173
Jun 14, 2026, 9:45 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- CapDitch sideShane Bergeron RC-181
Jun 14, 2026, 10:20 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- CapWorking sideSam Whitfield RC-388
Jun 14, 2026, 10:20 AM · logged by C. Ramirez (Survey)
WPS-1104-TI-11 Rev 1SMAW uphill 6G (fixed)E6010 / E7018-H4
4–36 in OD · wall 0.188–0.75 in · hardness 235 HV10 max
- RepairWorking sideRonnie Pace RC-547
Jun 14, 2026, 10:30 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
NDT results
- RTRepair
Jun 14, 2026, 8:00 PM · D. Halloran (ASNT II)
Material lamination in pipe body (mill defect, not charged)
Not charged to a welder.
Repairable indication — grind and re-weld authorized.
RT film map — clock position3 indications12123456789101112- UCUndercut12:49–12:52 · 0.34" · d 0.04"Within acceptance limits.
- UCUndercut1:18–1:28 · 1.05" · d 0.04"UC exceeds API 1104 acceptance limits — charged for re-work.
- EUExcess reinforcement3:19–3:23 · 0.42" · d 0.02"Within acceptance limits.
Call disputedOpen7/26/2026Kyle Bassett (Contractor QC) — Crew disputes the low cap call — cap reinforcement measured within API 1104 limits on the ditch side. Requesting Level III film review.
Escalated to NDT Level III · Curtis Vandergriff (NDT Level III (RT/UT))
Visual inspection (CWI)
API 1104 · Bevel, alignment and hi-lo verified prior to root.
API 1104
Coating inspection
No coating inspection recorded for this joint.