J-3120
repairRepair- Line
- LN-12
- Station
- 1872+00
- Weld date
- 2026-06-04
- Spec
- 24" × 0.375"
33.70320, -104.09720
No open cross-check alerts on this joint.
Welder passes
- RootDitch sideWeston Trahan RC-133
Jun 4, 2026, 8:35 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- RootWorking sideMarcus Cole RC-118
Jun 4, 2026, 8:35 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- Hot PassWorking sideBo Kinchen RC-146
Jun 4, 2026, 9:10 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- Hot PassDitch sideHector Ruiz RC-528
Jun 4, 2026, 9:10 AM · logged by C. Ramirez (Survey)
WPS-1104-TI-11 Rev 1SMAW uphill 6G (fixed)E6010 / E7018-H4
4–36 in OD · wall 0.188–0.75 in · hardness 235 HV10 max
- FillDitch sideSam Whitfield RC-388
Jun 4, 2026, 9:45 AM · logged by C. Ramirez (Survey)
WPS-1104-TI-11 Rev 1SMAW uphill 6G (fixed)E6010 / E7018-H4
4–36 in OD · wall 0.188–0.75 in · hardness 235 HV10 max
- FillWorking sideDale Whitcomb RC-533
Jun 4, 2026, 9:45 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- CapWorking sideSam Whitfield RC-388
Jun 4, 2026, 10:20 AM · logged by C. Ramirez (Survey)
WPS-1104-TI-11 Rev 1SMAW uphill 6G (fixed)E6010 / E7018-H4
4–36 in OD · wall 0.188–0.75 in · hardness 235 HV10 max
- CapDitch sideDale Whitcomb RC-533
Jun 4, 2026, 10:20 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- RepairWorking sideDale Whitcomb RC-533
Jun 4, 2026, 10:30 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
NDT results
- RTRepair
Jun 4, 2026, 8:00 PM · D. Halloran (ASNT II)
Moisture / weather-related porosity (not charged to welder)
Not charged to a welder.
Repairable indication — grind and re-weld authorized.
RT film map — clock position1 indication12123456789101112- IPIncomplete penetration8:23–8:32 · 0.91" · d 0.03"IP exceeds API 1104 acceptance limits — charged for re-work.
Visual inspection (CWI)
API 1104
Coating inspection
No coating inspection recorded for this joint.