J-2760
repairRepair- Line
- LN-12
- Station
- 1656+00
- Weld date
- 2026-06-01
- Spec
- 24" × 0.375"
33.48360, -103.89560
No open cross-check alerts on this joint.
Welder passes
- RootDitch sideOdell Rains RC-121
Jun 1, 2026, 8:35 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- RootWorking sideDwayne Ferris RC-204
Jun 1, 2026, 8:35 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- Hot PassWorking sideTravis Nolan RC-307
Jun 1, 2026, 9:10 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- Hot PassDitch sideHector Ruiz RC-528
Jun 1, 2026, 9:10 AM · logged by C. Ramirez (Survey)
WPS-1104-TI-11 Rev 1SMAW uphill 6G (fixed)E6010 / E7018-H4
4–36 in OD · wall 0.188–0.75 in · hardness 235 HV10 max
- FillDitch sideSam Whitfield RC-388
Jun 1, 2026, 9:45 AM · logged by C. Ramirez (Survey)
WPS-1104-TI-11 Rev 1SMAW uphill 6G (fixed)E6010 / E7018-H4
4–36 in OD · wall 0.188–0.75 in · hardness 235 HV10 max
- FillWorking sideDale Whitcomb RC-533
Jun 1, 2026, 9:45 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
- CapWorking sideKelly Boudreaux RC-350
Jun 1, 2026, 10:20 AM · logged by C. Ramirez (Survey)
WPS-1104-TI-11 Rev 1SMAW uphill 6G (fixed)E6010 / E7018-H4
4–36 in OD · wall 0.188–0.75 in · hardness 235 HV10 max
- CapDitch sideSam Whitfield RC-388
Jun 1, 2026, 10:20 AM · logged by C. Ramirez (Survey)
WPS-1104-TI-11 Rev 1SMAW uphill 6G (fixed)E6010 / E7018-H4
4–36 in OD · wall 0.188–0.75 in · hardness 235 HV10 max
- RepairWorking sideJesse Karr RC-455
Jun 1, 2026, 10:30 AM · logged by C. Ramirez (Survey)
WPS-1104-DH-01 Rev 2SMAW downhill 5G / 6GE6010 / E8010-G
6–36 in OD · wall 0.188–0.75 in · hardness 248 HV10 max
NDT results
- RTRepair
Jun 1, 2026, 8:00 PM · D. Halloran (ASNT II)
Material lamination in pipe body (mill defect, not charged)
Not charged to a welder.
Repairable indication — grind and re-weld authorized.
RT film map — clock position3 indications12123456789101112- PORPorosity4:31–4:34 · 0.36" · d 0.03"Within acceptance limits.
- UCUndercut5:12–5:34 · 2.28" · d 0.01"UC exceeds API 1104 acceptance limits — charged for re-work.
- SISlag inclusion11:02–11:06 · 0.40" · d 0.01"Within acceptance limits.
Visual inspection (CWI)
API 1104 · Root bead visual prior to hot pass.
API 1104
Coating inspection
No coating inspection recorded for this joint.