WeldGuard

Film QA review

Every indication plotted on film, grouped by defect code, so you can see where inspectors disagree on the same call.

Call consistency by code

CodeTotalRepair rate by inspectorSpread
LCLow capInconsistent521
  • D. Halloran (ASNT II)52%(148/284 · avg 0.69")
  • P. Estrada (ASNT II)0%(0/237 · avg 0.70")
52%
SISlag inclusion271
  • D. Halloran (ASNT II)15%(23/153 · avg 0.46")
  • P. Estrada (ASNT II)0%(0/118 · avg 0.30")
15%
UCUndercut308
  • D. Halloran (ASNT II)11%(19/175 · avg 0.44")
  • P. Estrada (ASNT II)0%(0/133 · avg 0.31")
11%
PORPorosity308
  • D. Halloran (ASNT II)6%(10/157 · avg 0.41")
  • P. Estrada (ASNT II)0%(0/151 · avg 0.29")
6%
EUExcess reinforcement252
  • P. Estrada (ASNT II)0%(0/128 · avg 0.30")
  • D. Halloran (ASNT II)0%(0/124 · avg 0.30")
0%
IFIncomplete fusion21
  • D. Halloran (ASNT II)100%(21/21 · avg 1.59")
0%
IPIncomplete penetration14
  • D. Halloran (ASNT II)100%(14/14 · avg 1.41")
0%
CRCrack2
  • P. Estrada (ASNT II)100%(2/2 · avg 1.95")
0%

Films with a disputed call (showing 0 recent indications)

No inconsistent calls detected across the current film set.